search  current discussion  categories  glazes - ash 

pecan hull ash glazes

updated fri 29 oct 04

 

Rhonda Kale on wed 27 oct 04


Digging around again and lo and behold-a sat 12 apr 97 posting by John McCain on clayart on pecan hull ash glazes-which goes to prove look once then go back and look again.....
http://www.potters.org/subject00716.htm

Rhonda Kale
31.23595 N, 85.40529 W
Potters Council Member
qndivauniv@earthlink.net

Gary Navarre on thu 28 oct 04


Re: pecan hull ash glazes
"Rhonda Kale" wrote:


Digging around again and lo and behold-a sat 12 apr 97 posting by John
McCain on clayart on pecan hull ash glazes-which goes to prove look once
then go back and look again..... http://www.potters.org/subject00716.htm

Rhonda Kale

Rhonda,
Looks like a job for the "Koie Ash Cooker",
http://public.fotki.com/GindaUP/ryoji_kioe_traditio/
especially with the ash being fine.
Good luck makin ash, keep going!

G.im Da U.P
Navarre Pottery
Norway, Michigan, USA

Maurice Weitman on thu 28 oct 04


At 6:22 AM -0500 on 10/28/04, gnavarre@uplogon.com wrote:
> Looks like a job for the "Koie Ash Cooker",
> http://public.fotki.com/GindaUP/ryoji_kioe_traditio/

I think you meant to say:

http://public.fotki.com/GindaUP/ryoji_koie_traditio/

Regards,
Maurice