search  current discussion  categories  people 

bisque firing ~ listen to ron roy,

updated fri 15 oct 04

 

william schran on thu 14 oct 04

and a question about 05 bisque

Kathy wrote ;>My understanding is that a cone 05 in the sitter is
likely closer to
an o6 on the shelf. Am I correct??<

If your kiln sitter is adjusted for this, it is true. But how would
you really know?

Only way to really be sure is to use witness cones on the kiln shelf,
even if you just used a ^06 self supporting cone by itself.

Bill