I have fooled around a little in the past with terra sigilata, with not
much success. I want to get serious about this one now. I have a small
ball mill. Can someone direct me to a method that will give really good
results and a fine burnished surface. Thanks.

Llewellyn Kouba
Abbey Pottery

Karen Hickson on wed 6 oct 04


This site has a very indepth recipe from Vince Pitelka. Hope this helps.
http://digitalfire.com/education/glaze/terasig.htm
Karen Hickson
Gainesville, FL



Llewellyn Kouba wrote:

> I have fooled around a little in the past with terra sigilata, with not
> much success. I want to get serious about this one now. I have a small
> ball mill. Can someone direct me to a method that will give really good
> results and a fine burnished surface. Thanks.
>
> Llewellyn Kouba
> Abbey Pottery
>
> ______________________________________________________________________________
>
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
> melpots@pclink.com.
>


--
"Life affords no higher pleasure than that of surmounting difficulties,
passing from one step of success to another, forming new wishes and seeing
them gratified." - Samuel Johnson

brian on wed 6 oct 04


On 5/10/04 Llewellyn wrote ....
>I have fooled around a little in the past with terra sigilata, with not
>much success.

"Near Enough is Good Enough for anything but Sigillata" was an
article I wrote a few years ago.
It would not qualify as the most authorative information on this
topic but might contain something that might help
There are a few illustrations too.

http://www.gartside.info/terrasigillatatext.htm

--
Brian Gartside
Pukekohe, New Zealand

Ivor and Olive Lewis on wed 6 oct 04


Dear Llewellyn Kouba,
Please do search Clayart Archive for Vince Pitelka's definitive
instructions on this one.
Best regards,
Ivor Lewis.
Redhill,
S. Australia.

Russel Fouts on thu 7 oct 04


-----------------------------

Date: Tue, 5 Oct 2004 10:15:31 -0600

>> I have fooled around a little in the past with terra sigilata, with not much success. I want to get serious about this one now. I have a small ball mill. Can someone direct me to a method that will give really good results and a fine burnished surface. Thanks. <<

http://users.skynet.be/russel.fouts/Files/Terra-Sig%20Primer.txt

Don't forget to have a look at the pots as well. Also check out the
Potters Portal, my links page.

Russel

--
Russel Fouts
Mes Potes & Mes Pots
Brussels, Belgium
Tel: +32 2 223 02 75
Mobile: +32 476 55 38 75

Http://www.mypots.com
Home of "The Potters Portal"
Over 1800 Pottery Links!
Updated frequently

"To announce that there must be no criticism of the president,
or that we are to stand by the president, right or wrong,
is not only unpatriotic and servile, but is morally treasonable
to the American public."

U.S. President (and Nobel Peace Prize winner) Theodore Roosevelt.