Hi,
I was wondering if any clayarters out there are familiar with Zen =
porcelain made by Mile High Clay in Denver. I got some on a trip there. =
I have used it only once and liked the way it threw. I didn't notice =
until after the pieces were dry that there was what looked like very =
small particles of sand throughout the clay. I was wondering if this is =
the normal composition of the clay? Anyone who is familiar with this =
clay body can maybe shed some light on it.