glaze mix question

updated mon 7 jun 04

 

Rob Byrne SA on sun 6 jun 04


Hi=20
I'm a new potter who is looking to mix a powder paint (stain / oxide) =
into a clear glaze base.
What ratio would work best and can i "sponge" the mixture onto my work.
Also - is it better to apply the mixture to greenware or bisque ware?

Would appreciate all recommendations and comments
with kind regards=20
Rob Byrne=20
South Africa =20




Attention: =20
This e-mail is privileged and confidential. If you are not the
intended recipient please delete the message and notify the sender.
Any views or opinions presented are solely those of the author.

william schran on sun 6 jun 04


Rob wrote">I'm a new potter who is looking to mix a powder paint
(stain / oxide) into a clear glaze base.
What ratio would work best and can i "sponge" the mixture onto my work.
Also - is it better to apply the mixture to greenware or bisque ware?<

Generally speaking, depending on the specific stain/oxide, a small
percentage is weighed and added dry to a weighed amount of dry glaze
base.
Can't provide a ratio that would work best unless you specify what
stain/oxide you will be using.
Better to sponge, or apply and other methods to bisqueware.