Imbolchottie@AOL.COM on wed 2 jun 04


Someone in my studio uses Soldate -- not sure about the number however.

From her firing I believe she bisques to ^09, then glazes to ^10.
This is done in a gas updraft so programming an electric kiln, geez, I don't
know.
Let me write her and ask.