Hi Ron,
Just wanted to let you know I had a glaze firing that went really well. =
I took your advice and loaded more loosely on the bottom and also slowed =
down the firing. The middle and top were right on cone 6 the bottom =
however was actually the hottest spot! Guess I loaded a little to =
light. Anyway I think I can work it out. Thank you for your help =
again. Also this was the first fire where I used Waterfall Brown and =
Variegated Slate Blue on more than just test tiles. I loved both of =
them!!
Loryn White

Ron Roy on thu 27 may 04


Hi Loryn,

Excellent! Thanks for letting me know.

RR


>Hi Ron,
>Just wanted to let you know I had a glaze firing that went really well. I
>took your advice and loaded more loosely on the bottom and also slowed
>down the firing. The middle and top were right on cone 6 the bottom
>however was actually the hottest spot! Guess I loaded a little to light.
>Anyway I think I can work it out. Thank you for your help again. Also
>this was the first fire where I used Waterfall Brown and Variegated Slate
>Blue on more than just test tiles. I loved both of them!!
>Loryn White