Hey Penni,

I have here a color chart from Coyote glaze company; I picked it up at =
NCECA. They have 3 different glazes that look yellow to me, but of =
course they're not CALLED yellow. One is "Iron Matt", one is "Clear" =
(although it's a soft butter yellow in the picture), and the last one is =
Yellow Orange. They are in New Mexico: (505) 344-2250

L



L. P. Skeen www.living-tree.net
Living Tree Pottery, Summerfield, NC
"There are three kinds of men. The ones who learn by reading, and the =
few who learn by observation. The rest of them have
to pee on the electric fence."------- Will Rogers (att.)