Daraburn@AOL.COM on sun 11 apr 04


Thanks Marc and John. I screened my glaze with 80 mesh, but only once. As I
look closely at the "dimples" in the glaze it seems the color around each is
a little whiter than the surrounding glaze so maybe I didn't mix well enough.
Also I sprayed these pieces, but I remember as I sprayed there were a few
raised pimple areas where the glaze was thicker. and I do think this is where the
dimples ended up. I will try adjusting the frit as John suggested and
screening more carefully. Thanks so much for your advice!

Dawn in Tennessee