search  current discussion  categories  techniques - stains 

=?iso-8859-1?q?re:=20=a0=20=a0=20=a0=20re:=20stains=20and=20stab?=

updated thu 8 apr 04

 

Susan Setley on wed 7 apr 04

=?ISO-8859-1?Q?le=20glazes?=

In a message dated 4/7/04 1:33:42 PM, alisa@CLAUSEN.MAIL.DK writes:


> I recently
> did this with Chrome again, and eeeks, no reds, nothing.=A0 I realize now
> that I did not put the Chrome in the glaze, but I also omitted the Tin.
> Have to keep sharp in the glaze lab.
>=20

It also pays to bring your bifocals. I once missed a decimal point and put i=
n=20
ten times as much cobalt as I should have in a Raku glaze. The results were=20
... UG-LEEEE!!!