linseed oil and unfired clay

updated sat 3 apr 04

 

Ivor and Olive Lewis on fri 2 apr 04


Dear Marie Gibbons,
This medium may have a long history under the name of Barbola Paste or
Barbotine.
It models well and hardens due to the property of Linseed oil
oxidising into a hard resin like material.
Best regards,
Ivor Lewis. Redhill, South Australia