search  current discussion  categories  glazes - misc 

use this for reglazing! it works great!

updated sun 28 mar 04

 

S.E.W. on fri 26 mar 04


I don't know if anyone mentioned "APT II" (that's APT 2) for reglazing =
and refiring. This stuff works great! Most ceramic supply stores carry =
it. It can be used for many things, not just reglazing, and that's what =
makes it so great. You add a couple of drops to your glaze and it makes =
the glaze adhere to the already fired glaze as if it was bisque! The =
piece doesn't need to be heated up either. I don't know what I would do =
without it. It is also used to mend greenware or to attach pieces =
together. You can add it to glaze instead of water to smooth out the =
consistency. The fact that it has so many uses is why I always keep this =
stuff around. If anyone has any questions, let me know!
Rachel