cone 06 bisque/cone 6 glaze: rachel

updated tue 23 mar 04


easley59 on mon 22 mar 04

I glaze my 06 bisque with a cone 6 glaze all the time.........where did =
you find your information? The clay is compatible with cone 6 glaze and =
it works just fine for me. some people do a cone 08 bisque with no =
probs. Have I been lucking out all these years?
Pam in Seattle