search  current discussion  categories  people 

leaky weapy result error and appoligies to ron roy

updated mon 23 feb 04

 

Lor & Jas White on sun 22 feb 04


Hi,
First I just wanted to apologize to RON Roy-I don't know why I wrote =
Rob--so sorry. Anyway I also need to change some of my test result =
findings. I went into the studio today and found some delayed crazing =
on my COE test tiles. B-mix showed crazing on glaze #4 579 after all =
although not heavily. Also Icelia showed delayed crazing on glaze #2 =
425. Learned my lesson of never throwing away test tiles!! =20

Loryn White