Ababi on tue 6 jan 04


Hello Russ
I use this recipe that Hal has sent us to worn you that not every recipe
you see on the net is worse trying.
In this recipe Hal went one step too far.
I read his recipes just for the fun; however if you are a new comer you
better learn first about new materials before you consider using them.
Try Monona Rossol book about safety in arts. It is called: The Artist's
Complete Health and Safety Guide.

The problem about these materials is not that they kill you - but the
misery you and your family might have in between.
Ababi Sharon
Glaze addict
Kibbutz Shoval Israel
ababisha@shoval.org.il
http://ababi.active.co.il
http://www.matrix2000.co.nz/Matrix%20Demo/Ababi.htm



-----Original Message-----
From: Clayart [mailto:CLAYART@LSV.CERAMICS.ORG] On Behalf Of Lou Roess
Sent: Tuesday, January 06, 2004 1:08 AM

Hal, could you maybe tell us what color these glazes are and whether
they
are gloss or matt?
Lou in Colorado