john b: use of calcined slips on bisque

updated wed 31 dec 03

 

piedpotterhamelin@COMCAST.NET on tue 30 dec 03


John
I assume that you are using Neph Sy on stoneware temp pots.
Unfortunately, the original post didn't mention the temp range so if it is for earthenware, he would need a soft frit.
Happy Holidays
Rick--
"Many a wiser men than I hath
gone to pot." 1649
> Rick,
>
> I use Bauer ship on bisque with the only adjustment being to apply it thin.
>
> I have also use Avery/Helmar slip which is 70 clay and 30 NS with no
> problems either. The thickness should be like skim milk though,
>
> Best of luck,
>
> John Britt
>