subject: thanks and underglaze question restated

updated tue 2 dec 03

 

Sandy Meadors on mon 1 dec 03


Thanks to everyone who answered my query about underglazes over, rather
than under, a base glaze. Lots of good feedback.
I realized I had not given a lot of information in my original post.
What I am wanting to do is dip the pieces in a white base glaze to make
the tan clay white, (I am using recycled) then use Laguna underglazes to
make
my designs........
......................................
What about painting your recycled clay with white slip, then use the
underglazes, then clear glaze?

Sandy Meadors