Leslie St. Clair on wed 26 nov 03


I was testing standard 225 clay recently and glazed
pieces with John & Ron's raw sienna and varigated
blue. Both pices dunted the day after I took them out
of the kiln. They were not being used in the oven. My
guess is that maybe those glazes don't fit the 225
body, and that could be the problem, not oven use.
but that's as far as I went with my testing, and I'm
wondering if anyone else has had the same problem.
Leslie St. Clair in Cincinnati, OH