Hi. I wonder if anyone would be willing to part with a white mat glaze
recipe for cone 04-03? appreciate any offers!--Thanks

Michele Jurist on sun 16 nov 03


Subject: White Mat Glaze


> Hi. I wonder if anyone would be willing to part with a white mat glaze
> recipe for cone 04-03? appreciate any offers!--Thanks



Hi:
This is a Richard Behren's recipe, if you have GB.

Gerstley Borate 18.2
Frit 3269 27.7
Alumina hydrate 5.4 (I use alumina oxide)
EPK 9
Silica 39.7

This produces a nice satin finish at ^05-04. I haven't tried it at a higher
temp. It takes oxides and stains well. If you are looking for a more mat
finish, e-mail me offlist and I will see what other recipes I may have.

Regards, Michele in Seattle

>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
>