good throwing clays/us kaolins

updated sat 27 sep 03

 

Craig Martell on fri 26 sep 03


Hello Again:

I said in my last post that most US Kaolins average about 1.5% titanium
oxide. OK, but I should have also mentioned that EPK is only about 0.33%
TiO2. It's the whitest of the bunch in my opinion.

regards, Craig Martell Hopewell, Oregon