search  current discussion  categories  glazes - misc 

glaze for week sept 22 rethought

updated mon 22 sep 03

 

Hal Mc Whinnie on sun 21 sep 03


BRIGHT TRANSPARENT COLEMANITE GLOSS
CONE 2-6
LITTLE FLUDITY
STAINS SHOW
BLUE MILKY WHITE
WHITE WERE THICK
SOURCE ALFRED

a-3 spar 42
colemanite 24
silica 15
zinc oxide 9
ept 4

analysis
k20 0.16
nao 0.06
mgo 0.05
cao 0.37
zno 0.37
al2o3 0.30
sio2 2.60
b2o3 0.50