canadian source for frit 3269 (p-25) for cone 6 metallic glaze

updated tue 23 sep 03

 

Eva Gallagher on sun 21 sep 03


Hi,
I am looking for a Canadian source of Frit 3269. PSH and Tuckers in =
Ontario do not carry it so wonder if there is any other supplier of it =
out there in Canada. Have not found anything on the Internet - though =
lots of US sources. I would like to use it in the metallic cone 6 glaze =
from Barbara Hanselmans' article listed in http://www.ceramicstoday.com/ =
. I tried Frits 3124 and 3134 and ended up with an interesting glaze =
especially over iron underglaze but not a metallic like in the article =
pictures. By the way I tried some of the other glazes in the article all =
with pretty good success - especially the Currie Blue.
Thanks,
Eva Gallagher, Deep River, Ontario, Canada=20

Tony Hansen on mon 22 sep 03


Check at www.ceramicmaterials.info for this
frit, there are lots of substitutes.

-------8<--------
Hi,
I am looking for a Canadian source of Frit 3269. PSH and Tuckers in =
Ontario do not carry it so wonder if there is any other supplier of it =
out there in Canada. Have not found anything on the Internet - though =
lots of US sources. I would like to use it in the metallic cone 6 glaze =
from Barbara Hanselmans\' article listed in http://www.ceramicstoday.com/ =
. I tried Frits 3124 and 3134 and ended up with an interesting glaze =
especially over iron underglaze but not a metallic like in the article =
pictures. By the way I tried some of the other glazes in the article all =
with pretty good success - especially the Currie Blue.
Thanks,
Eva Gallagher, Deep River, Ontario, Canada=20

______________________________________________________________________________
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.


--------
Tony Hansen, Digitalfire Corp.

Donald Burroughs on mon 22 sep 03


Eva try contacting The Sounding Stone here in Winnipeg. I purchase P-25
from them all the time. I believe they may even have Ferro 3269 as well.
Their telephone is 204.284.2964. They are open 10:00 am - 5:00 pm CST.

Don On the web @ http://www.autobahn.mb.ca/~donaldo