Steven D. Lee on mon 28 jul 03


My question is, "Can you mix Rasberry (which is a Chrome-Tin Red)
with other glazes without interfering with the Chrome-Tin red
interaction.

In other words, is I have a base of "Waterfall Brown" applied to a
piece and then have Rasberry on top will the waterfall brown
colorants and oxides prevent the chrome-tin from turning red?

***************************************************