search  current discussion  categories  wheels - misc 

wheel wandering

updated thu 3 jul 03

 

Lily Krakowski on wed 2 jul 03


Not back yet, but did glance at digests. Ok Years ago had same problem with
my Brent pedal--the adjustment of the red and green buttons did nothing
lasting. Then my husband discovered that the screw on the cross piece piece
was loose, and that whenever I pressed or released the pedal the cross piece
would "wander". Tightening that screw or nut or whatever solved Le
Problème.


Lili Krakowski
P.O. Box #1
Constableville, N.Y.
(315) 942-5916/ 397-2389

Be of good courage....