Dear Tom Sawyer,

I think your Redart Clay Slip Glaze is overdoing the Lithium compounds. =
You may recall that this is one of the ideal elements for reducing C of =
E.

If you do need to have a Lithium compound in that mixture to ensure the =
colour response, change to Petalite and use less of it. Try things out =
with a line blend of Redart/Petalite 95/5 down to 80/20. Leave the other =
one alone.

Best regards,

Ivor Lewis=20