search  current discussion  categories  glazes - misc 

: re: lowering glaze temp

updated mon 12 may 03

 

iandol on sat 10 may 03


Dear Brian Guffey,=20

Interesting to know that these felspars, which both contain K2O and =
Na2O, are Cone 10 fluxes. Yet you suggest Neph Sy which is a K2O-Na2O =
mineral.

I think Barry asked about getting rid of the out gassing from a sample =
glaze which had already fused well at cone 8 and which was suffering =
from blisters and pits. I cannot for the life of me see how changing =
melting fluxes will accomplish his objective.

Perhaps you could explain.

Best regards,

Ivor Lewis