grogged body glaze fit

updated sun 20 apr 03

 

Barry Salaberry on sat 19 apr 03


Hi All,

Does a claybody, when grog is added to it, change the way it fits a =
glaze?

If I take a clay body, and start adding grog in regular increments, will =
I eventually reach the point

where a given glaze, which fits the body (grog-free), will eventually =
start to craze?

Please reply off-list if this topic is too mundane or unworthy of the =
current philosophical elevation. Even=20

though I enjoy the current exchanges on NEA, I simply don't have the =
depth or fire to equal Elizabeth Priddy's

bulls-eyes or Kelly's petals of clarity.

Thanks if you can help,

Barry Salaberry

in Westbank, B.C.

planting Johnny-Jump-Ups, Sweet Alyssum and friends

for planters at the Farmer's Market this summer.