Megan Ratchford on thu 17 apr 03


Dear list,
Thank you to all who have responded to my massive quandary!! This =
list is amazing! I have worked on our raku glaze problem in isolation =
for months and have gotten nowhere. I have overlooked small details now =
blatantly obvious and have a new direction for me and my students to go =
in. I will try eliminating the borate in favor of a frit 3134 recipe =
using OM-4 ball clay instead of EPK and I will let the list know how =
this works. I know my glazes are far too high in Boron and now am able =
to use John's program to balance everything out!! Thank you clayart!!!
Megan Ratchford
In sunny and windy Colorado