Kat Valenzuela on mon 14 apr 03


I have noticed that there are some difference in various
talcs.
Does anyone know which one is a better flux in
a clay body? Silverline or Pioneer?

Kat in the Hat
kat@digitalfire.com

Ron Roy on fri 18 apr 03


Talcs vary quite a bit from brand to brand - better to get analysis of them
when deciding which to use as melters. I can help if I know what in em.

RR

>I have noticed that there are some difference in various
>talcs.
>Does anyone know which one is a better flux in
>a clay body? Silverline or Pioneer?
>
>Kat in the Hat
>kat@digitalfire.com

Ron Roy