Karim Motawi on sat 8 mar 03


Ron,
Where are we on that little glaze formulation project we started a few
weeks ago?
karim motawi

----- Original Message -----
From: Ron Roy
To:
Sent: Saturday, March 08, 2003 5:00 PM
Subject: Insight calculation course at Canador - July 03


> There will be a glaze calculation course (maybe 2) this summer at Canador
> College. The instructors will be Phil Yordy and Margaret Barlow for the
> first week.
> Margaret will do the 2nd week if there are enough students for two weeks
>
> I will be there for one day each week.
>
> Dates for the courses are
> July 7 -11 and July 14 to 18
> Fee is $220 plus material fee $37.45, residence accommodation for a week
for
> one person is $89.99 - these are in Canadian dollars.
>
> The brochure won't be back from the printer until end of March but the
> information should be on the web site soon. You can register over the net
> or by March 15. Here is the site:
>
> www.canadorec.on.ca
>
> Phil Yordy is a production potter and has been my assistant for the last
> two courses I gave there.
>
> Margaret has been teaching the glaze calc course at Mohawk College for
> several years now.
>
> Both are excellent teachers and bring a wealth of experience with them. I
> cannot stress enough how much I think of them both.
>
> Residence is in houses with 5 bedrooms and two Bathrooms - a kitchen and f
> ridge. Most students bring some pots and dishes and cook their own food.
> Breakfast and lunch are available at the college. The setting is beautiful
> - on a small lake outside NorthBay - it's about a 5 minute drive into town
> and there is bus service.
>
> You will be working in a computer lab and firing and mixing glazes in the
> pottery studio.
>
> Canador is about 200 miles north of Toronto and there is a shuttle service
> from Toronto Airport to the college.
>
> For those of you from USA this is a real bargain - a little over $200 Amr.
> for the course and accommodations.
>
> I will be away at NCECA and a holiday from the 12 to the 24th so if you
> have questions you can contact Margaret or Phil by email.
>
> "Margaret Barlow"
> "Phil & Jan Yordy"
>
> RR
>
> Ron Roy
> RR#4
> 15084 Little Lake Road
> Brighton, Ontario
> Canada
> K0K 1H0
> Phone: 613-475-9544
> Fax: 613-475-3513
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.