search  current discussion  categories  glazes - cone 8-10 

fw: ravenscrag at cone10

updated sat 8 mar 03

 

Sheldon Bieber on thu 6 mar 03


----- Original Message -----
From: Sheldon Bieber
To: Clayart
Sent: Thursday, March 06, 2003 5:49 PM
Subject: Ravenscrag at cone10


Hi,
The Ravenscrag slip glazes at cone 6 look great. Has anyone any formulas for cone 10 with Ravenscrag?
Shel

Charles Moore on fri 7 mar 03


Shel,

Check www.ravenscrag.com. You are supposed to be able to use Ravenscrag
slip as is at cone 10, perhaps adding up to 10% feldspar. Check out the
website.

Charles
Sacramento
----- Original Message -----
From: "Sheldon Bieber"
To:
Sent: Thursday, March 06, 2003 3:45 PM
Subject: Fw: Ravenscrag at cone10


> ----- Original Message -----
> From: Sheldon Bieber
> To: Clayart
> Sent: Thursday, March 06, 2003 5:49 PM
> Subject: Ravenscrag at cone10
>
>
> Hi,
> The Ravenscrag slip glazes at cone 6 look great. Has anyone any formulas
for cone 10 with Ravenscrag?
> Shel
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.