bobl@WIDOMAKER.COM on wed 5 mar 03


John,
Your postings on your website of the cone 6 glaze test results were very
helpful. I am using the Nutmeg and White Satin Matte with mixed results (so
far), and seeing your photos has really been a help, especially the cone
packs. I feel your results at about cone 7 were far superior to my slightly
underfired results. I refired, and things only got worse. I need to go
thicker and fire higher.
I never imagined Nutmeg and Licorice together. Nice combination.
I would love to see on ClayArt more links to photos of glaze test results.
Thanks for sharing yours.
Bob
Williamsburg, VA

June Perry on thu 6 mar 03


Bob,

I have a few pages of cone 6 test tile results with recipes and notations on
my web pages. Just go to my home page and scroll to the bottom of the page
for the cone 6 pages. I also have soda tests and C10 reduction tests,
soda/salt clay tests and oxide wash recipes on the website.

Regards,
June Perry
http://www.anglefire.com/art2/shambhalapottery/

Marcia Selsor on thu 6 mar 03


Dear June,
I went to the site under your signature 3 times and was sent to a dating
service "win today". My husband says that is a problem with angelfire.com
Best wishes,
marcia

June Perry wrote:
> Bob,
>
> I have a few pages of cone 6 test tile results with recipes and notations on
> my web pages. Just go to my home page and scroll to the bottom of the page
> for the cone 6 pages. I also have soda tests and C10 reduction tests,
> soda/salt clay tests and oxide wash recipes on the website.
>
> Regards,
> June Perry
> http://www.anglefire.com/art2/shambhalapottery/
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.
>


--
Tuscany in 2003
http://home.attbi.com/~m.selsor/Tuscany2003.html

Dai Scott on thu 6 mar 03


June, I don't know what's going on with either my computer or your website,
but when I click on your hot link, it takes me to something called WinToday,
which appears to be a dating site! I KNOW I've been to your site before,
and no problems then. Is anybody else having this problem?
Dai in Armstrong, BC

June's site:
> http://www.anglefire.com/art2/shambhalapottery/

Dewitt on thu 6 mar 03


At 09:59 3/6/03 -0800, you wrote:
>June, I don't know what's going on with either my computer or your website,
>but when I click on your hot link, it takes me to something called WinToday,
>which appears to be a dating site! I KNOW I've been to your site before,
>and no problems then. Is anybody else having this problem?
>Dai in Armstrong, BC
>
>June's site:
> > http://www.anglefire.com/art2/shambhalapottery/

It's a typo, try http://www.angelfire.com/art2/shambhalapottery/

deg

-------------------------------------------------------------------
Dewitt Gimblet It is better to know less, then to know
Austin, Tx so much that ain't so. - Josh Billings
-------------------------------------------------------------------