I'm looking for a cone 6 oxidation glaze.
Greatful for any response.
Robert Heiner, from the great state of Delaware

Ababi on fri 28 feb 03


Yes there is , I think it is of Behrens:
STONY FISSURED GLAZE
,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,

Cone 6 1222 deg.C. -
,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,

Cryolite 33.00
ULTROX 67.00
,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,

Seger Weight%
KNO 1.000 16.60%
Al2O3 0.333 9.09%
SiO2 1.514 24.36%
ZrO2 1.514 49.94%
Na2O 1.000 16.60%
Al:Si 4.54
Expan. 9.52
ST 330.92
Apply over a dark claybody
http://tinyclick.com/?60JFQZ
Ababi Sharon
Glaze addict
Kibbutz Shoval Israel
ababisha@shoval.org.il
http://members4.clubphoto.com/ababi306910/
http://www.milkywayceramics.com/cgallery/asharon.htm
and also
http://www.israel-ceramics.org/membersGallery/personalpage.asp?MID=507
---------- Original Message ----------

>I'm looking for a cone 6 oxidation glaze.
>Greatful for any response.
>Robert Heiner, from the great state of Delaware

>______________________________________________________________________________
>Send postings to clayart@lsv.ceramics.org

>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/

>Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.