the reason i made that alkaline glaze...

updated sat 1 feb 03

 

Ababi on fri 31 jan 03


..Was to remind you, the small bowl I got from Marta.
In fact I meant mainly to use it with RIO.
http://members4.clubphoto.com/ababi306910/472821/
The point was: To create in an electric kiln an appearance of soda glazed ware.
Therefore I sprayed thin layer.
Actually I did not go on - I was driven to other directions. A high alkaline glazes
without creasing is like a pizza without cheese!
Here is the recipe
ABABI'S SODA GLAZE FOR PORCELAIN - in electric kiln, defiantly a decorative glaze!
,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,

Cone 6 1222 deg.C. -
,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,

frit A 2120 45.00
kaolin CC31 30.00
FRIT 3701 25.00
,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,

Seger Weight%
KNO 0.790 17.31%
CaO 0.153 2.93%
MgO 0.005 0.06%
Li2O 0.053 0.54%
Al2O3 0.363 12.63%
B2O3 0.414 9.83%
SiO2 2.762 56.67%
TiO2 0.001 0.03%
K2O 0.054 1.74%
Na2O 0.736 15.57%
Al:Si 7.61
Expan. 10.72
ST 286.56
,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,
different % of RIO
in one case my dogmatic way of an add of: 3% BLACK COPPER OXIDE!
The reason I must repeat the test is one: This time I will sieve the glaze to have the
RIO spreads around though I am not sure it will be nicer.

Ababi Sharon
used to be pizza addict
Kibbutz Shoval Israel