Lily, how do these various forms of copper compare to one another and to
copper carbonate in terms of the color response they characteristically
produce?

Wanda

-----Original Message-----
From: Clayart [mailto:CLAYART@LSV.CERAMICS.ORG] On Behalf Of Lily
Krakowski
Sent: Friday, January 31, 2003 7:01 AM
To: CLAYART@LSV.CERAMICS.ORG
Subject: Re: Cobalt tricks

There IS black copper oxide (CuO) and it is pretty black. That is the
one
commonly used. There also is red copper oxide (Cu20) which is a lovely
wine color.