I am curious about how well the surface colours hold up over time. Do =
they fade (away from direct sunlight), do the colours reoxidize as =
happens with some raku work ? Is it a general practise to apply a =
sealant/wax ? MarjB

Maid O'Mud on sun 19 jan 03


My 1st pieces are about 5 years old and show no signs of fading. On some
I've used wax, others varathane, others left as is. No noticeable changes
:-)

Sam - Maid O'Mud Pottery
Melbourne, Ontario CANADA

"First, the clay told me what to do.
Then, I told the clay what to do.
Now, we co-operate."
sam 1994

http://www.ody.ca/~scuttell/

----- Original Message -----
From: "Marjorie"
To:
Sent: Saturday, January 18, 2003 1:06 PM
Subject: smoke firing question


I am curious about how well the surface colours hold up over time. Do they
fade (away from direct sunlight), do the colours reoxidize as happens with
some raku work ? Is it a general practise to apply a sealant/wax ? MarjB