i recycle clay by the ton it seems. in reality though, probably about
100 pounds a week. i have 2 bray trays (enormous plaster trays, hold 3-
5 gallon buckets o slop). they are fabulous and i usually have them
both in use. takes about 4 days to dry out the slop then off to my
venco pug. i love recycled clay. it stinks good and throws great
although sometimes a little short.

i saved buckets of slop for years so have enough backlogged for a very
long time. if i had more trays it would be gone.

my de-airing pug is one of my favorite "fancy" machines...makes me
happy.

take care,