glaze info needed.

updated sun 10 nov 02

 

Jim Brooks on fri 8 nov 02


I read a lot.. maybe to much.!!!. Recently, I came across a reference to
"Copper Yellow"... I have not found any more information about this.. Does
anyone know anything about copper yellows.. or can anyone point me in the
direction of more information?
Thanks Jim in Denton...

Lily Krakowski on fri 8 nov 02


Hands on I know little but I do think Hetherington had a lot, and so I
expect does Grebanier. Both likely to be at library.



Jim Brooks writes:

> I read a lot.. maybe to much.!!!. Recently, I came across a reference to
> "Copper Yellow"... I have not found any more information about this.. Does
> anyone know anything about copper yellows.. or can anyone point me in the
> direction of more information?
> Thanks Jim in Denton...
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.



Lili Krakowski
P.O. Box #1
Constableville, N.Y.
(315) 942-5916/ 397-2389

Be of good courage....

John Britt on sat 9 nov 02


Jim,

Hank Murrow has a recipe in Ian Curries "Revealing Glazes". I believe it
was high KNaO and Titanium with copper, but don't quote me.

John