RPeckham@COOKSONELECTRONICS.COM on fri 1 nov 02


Judy,
It is starting to get cold out. Is the heat running more. I remember
reading in a Bonsai book that in the winter some homes humidity level can
go down to around 10%. I think the book also compared that to 30%
humidity for the Sahara.

My last studio was forced hot air. Everything was fine in the spring,
summer, and fall, but in the winter everything cracked.

Randy Peckham
Listened to the leaves falling last night, sounded like rain.

Des & Jan Howard on sat 2 nov 02


Randy
Our area was at 31c temp & 7% humidity yesterday.
Great drying weather, our damp cupboards each 2 cubic metres
with concrete water ponds in the bottom need constant topups
& a close eye on the pots.
Jan just checked todays weather prediction, change coming,
with 32c temp & 58% humidity, yuck!!
Des

RPeckham@COOKSONELECTRONICS.COM wrote:

> Judy,
> It is starting to get cold out. Is the heat running more. I remember
> reading in a Bonsai book that in the winter some homes humidity level can
> go down to around 10%. I think the book also compared that to 30%
> humidity for the Sahara.

--

Des & Jan Howard
Lue Pottery
LUE NSW 2850
Australia
Ph/Fax 02 6373 6419
http://www.luepottery.hwy.com.au