Barbara on tue 29 oct 02


My problem is very close to Karen's, but I have an Olympic about 4 yrs old.
Good kiln, but I can't figure out how to candle it, etc.
Barb in Oregon
home of the 12'banding wheel !

----- Original Message -----
From: "Karen Sullivan"
To:
Sent: Tuesday, October 29, 2002 7:00 PM
Subject: skutt computer controlled kilns....yikes, help


> I do not seem to be able to track and
> figure out how to control the skutt electric kiln
> with the computer controls...touch pad...
>
> could someone walk me through the bisque,
> candle and then ramp to temperature phase.....
>
> I need the step by step setting sequence...
> of the kiln master controls....
> my goal is to candle for sixteen hours...
> I teach and want to start the candling process at
> the end of my teaching day....so 4 pm...
> and to begin firing the next morning at
> 8 am...I need help with the controls to fire
> the kiln in that process....
>
> many thanks
> karen
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
>
>