search  current discussion  categories  kilns & firing - raku 

liners/raku

updated thu 31 oct 02

 

mel jacobson on wed 30 oct 02


i should have said.
flu liners, wrapped in wire...sprayed
with four thin coats of itc.

they last a long, long, time.
mel

thanks tony.
From:
Minnetonka, Minnesota, U.S.A.
web site: my.pclink.com/~melpots
or try: http://www.pclink.com/melpots

Tony Ferguson on wed 30 oct 02


Mel,

Well why didn't you say ITC. 8-)

I may have to try that!

Thank you.

Tony Ferguson
On Lake Superior, where the sky meets the Lake

Stoneware, Porcelain, Raku
www.aquariusartgallery.com
218-727-6339
315 N. Lake Ave
Apt 312
Duluth, MN 55806


----- Original Message -----
From: "mel jacobson"
To:
Sent: Wednesday, October 30, 2002 8:29 AM
Subject: liners/raku


> i should have said.
> flu liners, wrapped in wire...sprayed
> with four thin coats of itc.
>
> they last a long, long, time.
> mel
>
> thanks tony.
> From:
> Minnetonka, Minnesota, U.S.A.
> web site: my.pclink.com/~melpots
> or try: http://www.pclink.com/melpots
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
>