Dear All,

Stephen Murfitt has asked me to pass on a list of corrections to his
glaze book; These are not Stephen's cock-ups, but alas; alterations made
at the printers!!

Glaze Book Corrections


Page 128: Top tile: should read: Recipe A applied over, not 50 / 50
Recipe B: plus 10 % red iron oxide

Page 128: Middle tile: Same changes as top tile

Page 128: Bottom tile: Should read: Recipe B plus 10% red iron oxide,
over Recipe C plus 10% red iron oxide, then recipe A applied over both.

Page 129: Bottom tile: should read: Recipe A over recipe B, plus 10% red
iron oxide.

Page 150: Middle tile: should read: Recipe A plus 3% rutile, over recipe
B plus 10% red iron oxide.

Page 172: Top tile: should read: Recipe A plus 3% rutile, over recipe B
plus 5% red iron oxide.

Page 268: Delete Cobalt Carbonate and Red Iron Oxide.

Steve Mills
Bath
UK