search  current discussion  categories  glazes - misc 

new page of soda/salt slip & glaze pictures and recipes added to my

updated sun 13 oct 02

 

June Perry on sat 12 oct 02

web site

I finally figured out the problem I was having uploading the pictures of the
tiles --- finally.
Now I'll be able to get on with getting some C10R glaze tiles scanned and
create those pages with the pictures and recipes.
Please note that the web site is a work in progress and not all links work on
all pages; but there is a home page, 4 pages of cone 6 test tiles with some
recipes, a page of soda/salt clay tests, two pages of soda/salt glaze and
slip tiles with recipes and a links page and two gallery pages.

If you just want to see the new page, just go to the bottoms of the home page
and hit the link that says: C10R SODA/SALT GLAZE GROUP #2

Here's a link to my web page.

Shambhala Pottery

If the link doesn't work, the page is:

http://www.angelfire.com/art2/shambhalapottery/index.html

Regards,