lewis red/blue

updated sat 28 sep 02

 

Deeclay@AOL.COM on fri 27 sep 02


I found a small amount of a glaze labeled "Lewis R/B" cone 10 reduction at
school. I did a test and it is a wonderful glossy denim blue that breaks red
where it is thick. Can't find the recipe for it anywhere. Has anyone ever
heard of it? I'm hoping someone will have the recipe for it and knows who
Lewis is.
Thanks in advance.
Diane in Sunny Miami (Broward Community College)