search  current discussion  categories  glazes - specific colors 

mel's any glaze blue

updated sun 22 sep 02

 

Kurt Wild on sat 21 sep 02


At 07:16 AM 9/21/02 -0500, MEL wrote:

>BLUE GLAZE:
>take any glaze formula/base
>add 1 percent cobalt.
>blue glaze.

That's going to make a hell of a strong blue glaze.
In my experience 0.25 to 0.5 percent has been plenty.

From my favorite chair - leg elevated, now in a short "walking" cast,
slowly getting better - laptop on my lap - phone at my side 715-425-5715
Kurt