Pat Southwood on fri 20 sep 02


Claybair ,

You were concerned about the lead? Sorry, it's my fault, I was using an =
abbreviation, Lead bisilicate is fritted.-65%PbO, 33% SiO2 and 2% Al2O3.
Pat.