search  current discussion  categories  kilns & firing - misc 

q: half loaded kiln

updated wed 4 sep 02

 

Lesley Alexander on tue 3 sep 02


Any opinions? Have to do a heavy reduction firing, updraft gas kiln,
half empty. Figure on loading it up with extra posts etc. Any other
ideas? Lesley celadon@silcom.com

Alistair Gillies on tue 3 sep 02


Hi
My instinct would be to load it as symmetrically as you can [even if
this is a 'false' load].


Alistair Gillies
Shropshire, England




In message <3D74E520.9506267F@silcom.com>, Lesley Alexander
writes
>Any opinions? Have to do a heavy reduction firing, updraft gas kiln,
>half empty. Figure on loading it up with extra posts etc. Any other
>ideas? Lesley celadon@silcom.com

Alistair Gillies
AGP Studio
01952 882909
07973 866198

www.agpstudio.co.uk [The builders are _still_ working]