I am looking for the Raku glaze, Fatty White Crackle.
I was told it was on www.mdc.net, but I can't get that site. The glaze is
just what the name implies and is beautiful. I hope someone out there can
help me.
Thanks,
Martha G.

Dewitt on thu 29 aug 02


At 22:58 8/28/02 -0400, Clayhannie@AOL.COM wrote:
>I am looking for the Raku glaze, Fatty White Crackle.
> I was told it was on www.mdc.net, but I can't get that site. The glaze is
>just what the name implies and is beautiful. I hope someone out there can
>help me.
>Thanks,
>Martha G.

Try http://www.dinoclay.com/info/glazes/degraku.html.

deg

Karen Shapiro on thu 29 aug 02


Here's the "Fatty White Crackle":

frit 3134 - 160/ ball clay - 18/ silica - 18/ zircopax - 20

it is a lovely glaze.

Karen in Gualala



---------------------------------