paperclay with an add of 1% brass chips

updated mon 19 aug 02

 

Ababi on sun 18 aug 02


Please visit my paperclay page the last six slides:
http://members4.clubphoto.com/ababi306910/803792/
Stoneware as paperclay with an add of 1% brass chips as ^6 ox as well as raku
Ababi