Does anyone have a standard number of lbs of clay for a regular coffee mug,
and say a double coffee mug?


Randy

Des & Jan Howard on sun 18 aug 02


Randy
For thrown mugs:
380 ml finished capacity - 325 g clay - thrown to 95 mm H x 95 mm D.
470 ml finished capacity - 450 g clay - thrown to 120 mm H x 100 mm D.
Des

ranmcc wrote:

> Does anyone have a standard number of lbs of clay for a regular coffee mug,
> and say a double coffee mug?

--